Liang-Wen Ji، نويسنده , , Chih-Ming Lin، نويسنده , , Te-Hua Fang، نويسنده , , Tung-Te Chu، نويسنده , , Huilin Jiang، نويسنده , , Wei-Shun Shi، نويسنده , , Cheng-Zhi Wu، نويسنده , , Tian-Long Chang، نويسنده , , Teen-Hang Meen، نويسنده , , Jingchang Zhong، نويسنده ,
Abstract :
ZnO nanorod arrays were synthesized by chemical-liquid deposition techniques on MgxZn1−xO (x = 0, 0.07 and 0.15) buffer layers. It is found that varying the Mg concentration could control the diameter, vertical alignment, crystallization, and density of the ZnO nanorods. The X-ray diffraction (XRD), transmission electron microscopy (TEM), and selected area electron diffraction (SAED) data show the ZnO nanorods prefer to grow in the (0 0 2) c-axis direction better with a larger Mg concentration. The photoluminescence (PL) spectra of ZnO nanorods exhibit that the ultraviolet (UV) emission becomes stronger and the defect emission becomes weaker by increasing the Mg concentration in MgxZn1−xO buffer layers.
Keywords :
ZnO nanorods , Chemical-liquid deposition , Photoluminescence , MgxZn1?xO , Sol–gel