• Title of article

    Synthesis of LiCo0.3Ni0.7O2 by using β-Co0.3Ni0.7OOH and LiOH·H2O as starting materials

  • Author/Authors

    Tong Dong-Ge، نويسنده , , Lai Qiong Yu، نويسنده , , Wei Ni-Ni، نويسنده , , Ji Xiao Yang، نويسنده ,

  • Issue Information
    دوهفته نامه با شماره پیاپی سال 2006
  • Pages
    5
  • From page
    124
  • To page
    128
  • Abstract
    LiCo0.3Ni0.7O2 has been prepared at 700 °C for 8 h in air by using β-Co0.3Ni0.7OOH and LiOH·H2O as starting materials. The sample was characterized by XRD, ICP, SEM, XPS, valence analysis and electrochemical performance. The results show that the sample has a good layered structure and the average oxidation value of (Co, Ni) in the sample is +3. Moreover, the sample has a good electrochemical performance with an initial discharge capacity of 145 mAh g−1 and a good capacity retention of 97.79% after 50 cycles. The good cycle performance is attributed to the limited structural disorder and the non-occurrences of any structural transition from hexagonal to monoclinic during the charge and discharge processes.
  • Keywords
    Synthesis , Cathode materials , LiCo0.3Ni0.7O2 , ?-Co0.3Ni0.7OOH , Lithium ion batteries
  • Journal title
    Materials Chemistry and Physics
  • Serial Year
    2006
  • Journal title
    Materials Chemistry and Physics
  • Record number