Title of article :
Microstructure and superplasticity of laser welded Ti–6Al–4V alloy
Author/Authors :
Donghai Cheng، نويسنده , , JIHUA HUANG، نويسنده , , Xingke Zhao، نويسنده , , Hua Zhang، نويسنده ,
Issue Information :
ماهنامه با شماره پیاپی سال 2010
Pages :
4
From page :
620
To page :
623
Abstract :
In this paper laser beam welding (LBW) was used to join Ti–6Al–4V alloy as a pre-forming operation before superplastic deformation (SPF) process. Superplastic deformation behavior of laser welded Ti–6Al–4V alloy was investigated. The results indicated that the welded Ti–6Al–4V alloy had good superplasticity when deformed at temperature range of 870–920 °C and strain rate range of 10−3–10−2 s−1, and the elongation was 233–397%. The microstructure observation indicated that dynamic recrystallization happened in the weld bead, and the acicular structure of weld bead was transforming into equiaxed grains during tensile process.
Journal title :
Materials and Design
Serial Year :
2010
Journal title :
Materials and Design
Record number :
1068644
Link To Document :