Ceramic ZrO2 and metallic Ti–6Al–4V alloy are jointed by using a Ti33Zr17Cu50 (at.%) amorphous alloy as a solder at 1123–1273 K in a high vacuum. It is demonstrated that the microstructure and mechanical properties are significantly influenced by the brazing temperature, the heat time and the cooling rate. The brazing seam jointing ZrO2 with Ti–6Al–4V is composed of ZrO2/Cu2Ti4O, (Ti,Zr)2Cu/TiO, Ti2O/CuTi2, (Ti,Zr)2Cu/CuTi2/Ti–6Al–4V alloys and compounds, of which the increasing thickness weakens the shear strength as the brazing temperature, the heat time the cooling rate increase. The maximum shear strength of the brazing joints reaches 162 MPa with the optimal technical parameters: the brazing temperature of 1173 K, the heat time of 10 min and the cooling rate of 5 K/min. The fracture of the joint occurs in the brittle seam layer nearby the side of ZrO2.
Journal title :
Materials and Design
Serial Year :
2013
Journal title :
Materials and Design
Record number :
1073026
Link To Document :
بازگشت