    An experimental parameter of cavitation erosion resistance for TiN coatings

  • Author/Authors

    Alicja Krella، نويسنده ,

  • Issue Information
    ماهنامه با شماره پیاپی سال 2011
  • Pages
    6
  • From page
    252
  • To page
    257
  • Abstract
    A series of cavitation erosion tests were carried out to investigate the resistance of the TiN coatings against cavitation action. The TiN coatings were deposited at various deposition parameters on austenitic stainless steel, X6CrNiTi18-10, with various coating thicknesses by means of the cathodic arc evaporation method (CAVD). Investigations were performed in a cavitation tunnel with a slot cavitator. The estimation of cavitation resistance of the TiN coatings was performed on the basis of the incubation period and the mass loss. The investigations show that coating hardness, Youngʹs modulus, adhesion and coating thickness have an influence on coating endurance to cavitation degradation. The parameter H·LC2/E·h1/2 shows very good fitting to data points (R2 = 0.9707). Along with the increase of the H·LC2/E·h1/2 parameter the mass loss decreases indicating a continuous improvement in the cavitation erosion resistance.
  • Keywords
    Fracture , TiN coatings , Adhesion , Impact , Cavitation erosion , Hardness
  • Journal title
    Wear
  • Serial Year
    2011
  • Journal title
    Wear
  • Record number

    1091852