Author/Authors :
Sizhong Li، نويسنده , , Quangui Guo، نويسنده , , Yan Song، نويسنده , , Jingli Shi، نويسنده , , Lang Liu، نويسنده ,
Abstract :
Carbon foams with high thermal conductivity were obtained from mixtures of mesophase pitch and pitch fluoride. The addition of pitch fluoride in mesophase pitch could significantly increase the specific thermal conductivity of as-prepared carbon foams. After graphitization at 2873 K, the specific thermal conductivity of carbon foams increased from 82 up to 155.4 (W/mK)/(g/cm3) when the content of pitch fluoride was 3% in the raw material.