• Title of article

    Degradation of hydrogen absorbing capacity in cyclically hydrogenated TiMn2 Original Research Article

  • Author/Authors

    Satoshi Semboshi، نويسنده , , N Masahashi، نويسنده , , S Hanada، نويسنده ,

  • Issue Information
    دوهفته نامه با شماره پیاپی سال 2001
  • Pages
    9
  • From page
    927
  • To page
    935
  • Abstract
    Degradation of the hydrogen absorbing capacity in cyclically hydrogenated TiMn2 (Ti–60 at.% Mn) with Laves structure was studied by measurement of pressure–composition–isotherm (PCT) curves, X-ray diffraction and microstructure observation. Characteristic changes with cyclic hydrogenation are observed as follows. The hydrogen absorbing capacity remarkably decreases, the lattice constant increases, the amount of hydrogen retained in TiMn2 increases and it approaches almost zero by dehydrogenation at 673 K in vacuum. Nano-sized regions with Moiré patterns are produced in TiMn2 with hydrogenation and Debye rings corresponding to titanium hydride δ-TiH appear in the diffraction pattern. Based on these observations it is concluded that the degradation of hydrogen absorbing capacity after cyclic hydrogenation is attributable to the introduction of retained hydrogen, heterogeneous strain and/or nano-sized regions.
  • Keywords
    Hydride , Microstructure , X-ray diffraction (XRD) , Titanium alloys , Transmission electron microscopy (TEM)
  • Journal title
    ACTA Materialia
  • Serial Year
    2001
  • Journal title
    ACTA Materialia
  • Record number

    1142150