Title of article
Coking and deactivation during n-hexane cracking in ultrastable zeolite Y Original Research Article
Author/Authors
Boontham Paweewan، نويسنده , , Patrick J. Barrie، نويسنده , , Lynn F. Gladden، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 1999
Pages
10
From page
259
To page
268
Abstract
A multi-technique approach has been used to investigate coke formation and the effects of coke formation during n-hexane cracking on ultrastable zeolite Y. The product analysis reveals that propane and propene are the major products, and this suggests that the reaction initiation step may be direct protonation at very strong Brønsted acid sites. The coke formed does not change in composition significantly over the course of the reaction. Infrared spectroscopy reveals that the vast majority of Brønsted and Lewis acid sites are still present in the catalyst, even when the catalyst activity has become low. Diffusion measurements using pulsed field gradient (PFG) NMR show that the mobility of adsorbed n-butane or n-hexane is not affected by the presence of the coke, and so shows that pore blockage is not a significant factor. Based on the experimental results, it is argued that selective site poisoning of a few very strong acid sites is the main deactivation mechanism for this reaction under the conditions employed.
Keywords
Cracking , Zeolite Y , Poisoning , selective site , Coking , Deactivation
Journal title
Applied Catalysis A:General
Serial Year
1999
Journal title
Applied Catalysis A:General
Record number
1149828
Link To Document