• Title of article

    Oxidative steam reforming of methane under atmospheric and pressurized conditions over Pd/NiO–MgO solid solution catalysts Original Research Article

  • Author/Authors

    Mohammad Nurunnabi، نويسنده , , Yuya Mukainakano، نويسنده , , Shigeru Kado، نويسنده , , Tomohisa Miyazawa، نويسنده , , Kazu Okumura c، نويسنده , , Toshihiro Miyao، نويسنده , , Shuichi Naito، نويسنده , , Kimihito Suzuki، نويسنده , , Ken-ichiro Fujimoto، نويسنده , , Kimio Kunimori، نويسنده , , Keiichi Tomishige، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2006
  • Pages
    12
  • From page
    1
  • To page
    12
  • Abstract
    The effect of the Pd loading in NiO–MgO solid solution was investigated in oxidative steam reforming of methane under atmospheric and pressurized conditions. The small amounts of Pd addition on Ni0.2Mg0.8O can inhibit the oxidation of Ni species and the mixture can maintain the reforming ability at low W/F conditions under atmospheric pressure, where Ni0.2Mg0.8O catalyst deactivated. In addition, Ni0.2Mg0.8O catalyst improved remarkably, gaining both high activity and excellent stability by the addition of small amounts of Pd under pressurized conditions. The deactivation rate was closely related to the amount of deposited carbon. Characterization results of TEM, TPR, EXAFS and FTIR suggest that Pd–Ni alloy particles are formed on Pd/Ni0.2Mg0.8O catalysts. The Pd–Ni alloy particles with a low ratio of Pd to Ni can play an important role in the high resistance to carbon deposition.
  • Keywords
    Oxidative reforming , Steam reforming , Methane , NiO–MgO solid solution , Deactivation , Carbon deposition , Pd
  • Journal title
    Applied Catalysis A:General
  • Serial Year
    2006
  • Journal title
    Applied Catalysis A:General
  • Record number

    1152734