Title of article :
Thermal degradation of coordination polymer [Cd(N-Boc-gly)2(H2O)2]n
Author/Authors :
Maja T. ?umar-Ristovi?، نويسنده , , Katarina K. An?elkovi?، نويسنده , , Dejan Poleti، نويسنده , , Dragica M. Mini?، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2011
Pages :
6
From page :
25
To page :
30
Abstract :
Multi-step thermal degradation of coordination polymer [Cd(N-Boc-gly)2(H2O)2]n in non-isothermal conditions was studied. The kinetic parameters were determined from the thermal decomposition data using the isoconversion and non-isoconversion techniques. It was shown that the coordination polymer is stable up to 60 °C, when the multi-step process of thermal dehydration, followed by steps of degradation, starts. The kinetic triplet for the step of dehydration was established as image, Einv = 170.4 ± 6.4 kJ mol−1 and Zinv = 2.6 × 1023. The established kinetic model, known as “D3 model”, was confirmed by application criteria defined by Màlek, Perez-Maqueda et al. as well as Master plot method. Dehydration step is followed by two steps of dehydrated coordination polymer degradation. On the base of the dependence of Arrhenius parameters (Ea and Z) on conversion degree (α), the mechanisms of degradation were discussed. In this way it was shown that second and third steps of degradation of coordination polymer are complex involving more than one elementary step. The second step corresponds to the loss of two C6H5CH2O– fragments in two parallel steps. The third step of degradation, ascribed to the loss of two –C(double bond; length as m-dashO)NHCH2– fragments, is complicated by changing kinetically to diffusion control.
Keywords :
Coordination polymer , Non isothermal kinetics , Thermal degradation kinetics
Journal title :
Thermochimica Acta
Serial Year :
2011
Journal title :
Thermochimica Acta
Record number :
1199817
Link To Document :
بازگشت