Title of article
Synthesis and characterization of Eu2+ activated X12Al10.6Si3.4O32Cl5.4 (X=Sr,Ca) phosphors
Author/Authors
V.B. Pawade، نويسنده , , N.S. Dhoble، نويسنده , , S.J. Dhoble، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2012
Pages
5
From page
2054
To page
2058
Abstract
In this article, we have reported emission characteristics of Eu2+ activated Sr12Al10.6Si3.4O32Cl5.4 and Ca12Al10.6Si3.4O32Cl5.4 phosphors, prepared by combustion synthesis. The PL excitation was monitored at two different wavelengths 254 nm (mercury excitation) and 354 nm (mercury free excitation), which shows broad-blue emission bands at 432 nm, and 438 nm for 354 nm excitation wavelength. Under mercury excitation at 254 nm it shows emission wavelengths at 470 nm, 589 nm, 592 nm, and 617 nm for the prepared Sr12Al10.6Si3.4O32Cl5.4 and Ca12Al10.6Si3.4O32Cl5.4 phosphors. Further it was characterized by XRD, for the investigation of phase and purity of the phosphors. Thermal degradation of the phosphors was also studied at different temperatures.
Keywords
Combustion synthesis , thermal degradation , XRD , Phosphor , Photoluminescence
Journal title
Journal of Luminescence
Serial Year
2012
Journal title
Journal of Luminescence
Record number
1261294
Link To Document