Title of article :
Sintering and oxidation resistance of compositions in the SiC–La2O3–Al2O3–Cr2O3 system I. Pressureless sintering of compositions in the SiC–La2O3–Al2O3–Cr2O3 system at low temperatures
Author/Authors :
Andrei Kirianov، نويسنده , , Akira Yamaguchi، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2000
Pages :
6
From page :
441
To page :
446
Abstract :
Sintering of materials, which were prepared from β-SiC and LaCrO3 with Al2O3, β-SiC and LaAlO3, β-SiC and LaAlO3 with Cr2O3 and Al2O3 via heating at 1700°C in graphite powder, was studied. Significant densification of material was achieved in SiC–LaCrO3–Al2O3 composition due to a formation of liquid phase. The formation of liquid phase is considered to be promoted by a reaction of chromium oxide with starting components. SiC–LaCrO3–Al2O3 compositions were sintered to about 90% of theoretical density at 1700°C. The material had a structure comprising a matrix made up of SiC grain with tiny LaAlO3 crystals and 2–4 μm inclusions of chromium carbide. As result, the material showed improved fracture toughness of 5 MPa m1/2 compared to that of SiC.
Keywords :
D. SiC , D. Al2O3 , LaCrO3 , A. Sintering , D. Carbides
Journal title :
Ceramics International
Serial Year :
2000
Journal title :
Ceramics International
Record number :
1268186
Link To Document :
بازگشت