Title of article :
Effect of heating rate on microstructure and properties of spark plasma sintered Li-α-sialon
Author/Authors :
Zhangfu Yang، نويسنده , , Hao Wang، نويسنده , , Xinmin Min، نويسنده , , Weimin Wang، نويسنده , , Zhengyi Fu، نويسنده , , Soo Wohn Lee، نويسنده , , Tohru Sekino and Koichi Niihara، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2011
Pages :
6
From page :
2175
To page :
2180
Abstract :
Li-α-sialon ceramics with low oxygen content were prepared by spark plasma sintering at 1750 °C, using three heating rates of 100 °C/min, 200 °C/min and 300 °C/min. In all cases, the densification of Li-α-sialon ceramics is effectively promoted. The rapidly anisotropic growth of grains, either α-sialon or β-sialon, is significantly enhanced with a heating rate above 200 °C/min. This could be attributed to a large amount of low viscosity oxygen-rich liquid formed at elevated temperatures, which gives rise to a so-called dynamic ripening mechanism at the early stage of sintering. Furthermore, for the composition near α-sialon boundary, the oxygen-rich liquid results in the formation of β-sialon together with a large amount of intergranular glassy phase. Only the Li-doped sialon with low lithium and oxygen content possesses relatively high infrared transmittance when sintered at a rate of 100 °C/min.
Keywords :
A. Sintering , C. Optical properties , D. Sialon , B. Microstructure-final
Journal title :
Ceramics International
Serial Year :
2011
Journal title :
Ceramics International
Record number :
1273413
Link To Document :
بازگشت