    Diffusivity, activity and solubility of oxygen in liquid lead and lead–bismuth eutectic alloy by electrochemical methods

  • Author/Authors

    Ganesan، نويسنده , , Rajesh and Gnanasekaran، نويسنده , , T. and Srinivasa، نويسنده , , Raman S. Srinivasa، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2006
  • Pages
    17
  • From page
    133
  • To page
    149
  • Abstract
    The diffusivity of oxygen in liquid lead and lead–bismuth eutectic (LBE) alloy was measured by a potentiostatic method and is given by log ( D O Pb / cm 2 s - 1 ) = - 2.554 - 2384 / T ( ± 0.070 ) , 818–1061 K, and log ( D O LBE / cm 2 s - 1 ) = - 0.813 - 3612 / T ( ± 0.091 ) , 811–980 K. The activity of oxygen in lead and LBE was determined by coulometric titration experiments. Using the measured data, the standard free energy of dissolution of oxygen in liquid lead and LBE was derived and is given by G O ( Pb ) xs = - 121 349 + 16.906 T ( ± 560 ) J ( g atom O ) - 1 , 815 – 1090 K , G O ( LBE ) xs = - 127 398 + 27.938 T ( ± 717 ) J ( g atom O ) - 1 , 812 – 1012 K . Using the above data, the Gibbs energy of formation of PbO(s) and equilibrium oxygen pressures measured over the oxygen-saturated LBE alloy, the solubility of oxygen in liquid lead and LBE were derived. The solubility of oxygen in liquid lead and LBE are given by log(S/at.%O) = −5100/T + 4.32 (±0.04), 815–1090 K and log(S/at.%O) = −4287/T + 3.53 (±0.06), 812–1012 K respectively.
  • Journal title
    Journal of Nuclear Materials
  • Serial Year
    2006
  • Journal title
    Journal of Nuclear Materials
  • Record number

    1363041