Threshold stress intensity factor for delayed hydride cracking of a recrystallized N18 alloy plate along the rolling direction
Author/Authors :
Sun، نويسنده , , Chao and Tan، نويسنده , , Jun and Ying، نويسنده , , Shihao and Peng، نويسنده , , Qian and Li، نويسنده , , Cong، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2010
Pages :
6
From page :
212
To page :
217
Abstract :
The objective of this study is to obtain the threshold stress intensity factor, KIH, for an initiation of delayed hydride cracking in a recrystallized N18 (Zr–Sn–Nb–Fe–Cr) alloy plate which was manufactured in China, gaseously charged with 60 ppm of hydrogen by weight. By using both the load increasing method and load drop method, the KIH’s along the rolling direction were investigated over a temperature range of 150–255 °C. The results showed that KIH along the rolling direction was found to be higher in the load increasing method than that in the load drop method. In the load increasing method, KIH’s of the N18 alloy plate appeared to be in the range of 31 – 32.5 MPa m , and KIH in the load drop method appeared to be in the range of 27.5 – 28.6 MPa m . This means that the N18 alloy plate has high tolerance for DHC initiation along the rolling direction. The texture of a N18 alloy plate was investigated using an X-ray diffraction and the KIH was discussed based on texture and analytically as a function of the tilting angle of hydride habit planes to the cracking plane.
Journal title :
Journal of Nuclear Materials
Serial Year :
2010
Journal title :
Journal of Nuclear Materials
Record number :
1363505
Link To Document :
بازگشت