Abstract :
The formation of radial cracks from Vickers indentations on the surfaces of both unirradiated and irradiated samples of (As1 − xBix)2Se3 glasses with x ≤ 0.1 is investigated as a function of indentation load P. It was found that radial cracks around indentations are produced on the surfaces of all samples at loads exceeding a particular applied load Pcapp but this threshold load is higher by a factor of 15 to 30 from the value of Pc calculated from the theoretical dependence of ratio c/d of crack length c measured from the center of indentation impression to indentation impression diagonal d on applied load P. By fitting the experimental P(c3/2) data in an expression relating c and P according to expanding cavity for elastic/plastic solid and from a theoretical expression relating load-independent hardness H and threshold load Pc for crack formation estimated from the experimental data of the dependence of c/d on P, the value of indentation fracture toughness KC of As2Se3 glasses, irrespective of Bi content in the samples and their irradiation, was found to be about 0.52 MPa⋅m1/2.
Keywords :
fracture toughness , Indentation hardness , Indentation cracks , Arsenic selenide glasses
Journal title :
Journal of Non-Crystalline Solids
Serial Year :
2011
Journal title :
Journal of Non-Crystalline Solids
Record number :
1379749
Link To Document :
بازگشت