    Densification of nanocrystalline Y2O3 ceramic powder by spark plasma sintering

  • Author/Authors

    Chaim، نويسنده , , Rachman and Shlayer، نويسنده , , Amit and Estournes، نويسنده , , Claude، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2009
  • Pages
    8
  • From page
    91
  • To page
    98
  • Abstract
    Nanocrystalline Y2O3 powders with 18 nm crystallite size were sintered using spark plasma sintering (SPS) at different conditions between 1100 and 1600 °C. Dense specimens were fabricated at 100 MPa and 1400 °C for 5 min duration. A maximum in density was observed at 1400 °C. The grain size continuously increased with the SPS temperature into the micrometer size range. The maximum in density arises from competition between densification and grain growth. Retarded densification above 1400 °C is associated with enhanced grain growth that resulted in residual pores within the grains. Analysis of the grain growth kinetics resulted in activation energy of 150 kJ mol−1 and associated diffusion coefficients higher by 103 than expected for Y3+ grain boundary diffusion. The enhanced diffusion may be explained by combined surface diffusion and particle coarsening during the heating up with grain boundary diffusion at the SPS temperature.
  • Keywords
    Densification , spark plasma sintering , Nanocrystalline , grain growth , Y2O3
  • Journal title
    Journal of the European Ceramic Society
  • Serial Year
    2009