    The effect of annealing at 1400 °C on the structural evolution of porous C-rich silicon (boron)oxycarbide glass

  • Author/Authors

    Sorarù، نويسنده , , Gian Domenico and Pena-Alonso، نويسنده , , Raquel and Kleebe، نويسنده , , Hans-Joachim، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2012
  • Pages
    7
  • From page
    1751
  • To page
    1757
  • Abstract
    A precursor SiBOC glass was annealed at 1400 °C for 1, 3, 5 and 10 h and then it was HF etched in order to dissolve the SiO2/B2O3 phase and to obtain a porous C-rich oxycarbide glass. The porous material was studied by N2 absorption. The pore diameter of the porous C-rich SiBOC glass ranges between 2 and 5 nm and continuously increases with increasing annealing time. The pore volume also increases with the annealing time up to ≈1.0 cm3/g which is close to the pore volume estimated from the chemical composition (1.04 cm3/g) assuming complete dissolution of the silica-based phase.
  • Keywords
    A. Precursors-organic , D. Carbon , Polymer-derived ceramics , D. SiO2 , D. SiC