    Absorption tails and extinction in luminescent solar concentrators

  • Author/Authors

    Earp، نويسنده , , Alan A. and Franklin، نويسنده , , Jim B. and Smith، نويسنده , , Geoff B.، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2011
  • Pages
    6
  • From page
    1157
  • To page
    1162
  • Abstract
    Non-ultraviolet (UV) photoexposure of luminescent solar concentrators (LSCʹs) can produce photoproducts that cause additional extinction at wavelengths somewhat longer than the main dye absorption peak. This photo-induced ‘tails’ extinction is deleterious to luminous output in collectors of useful lengths. An experimental method that enables the subdivision of tails extinction in an LSC into absorbed and scattered components is described. The relevant theory is outlined, and experimental results are presented for a polymethyl methacrylate (PMMA) LSC containing Lumogen F083 dye. For this sample, tails absorption increased significantly with outdoor exposure, while tails scattering remained constant. Further measurements indicate that LSC luminous output is around five times more sensitive to tails absorption than to fluorescence quenching. This work also indicates that merely checking for dye quenching, as is often done, can be a misleading indicator of long-term LSC output.
  • Keywords
    extinction , Light transport , Photodegradation , fluorescence , PMMA , Luminescent solar concentrators
  • Journal title
    Solar Energy Materials and Solar Cells
  • Serial Year
    2011
  • Journal title
    Solar Energy Materials and Solar Cells
  • Record number

    1485383