Internal friction in Fe–Al–Si alloys at elevated temperatures
Author/Authors
Pavlova، نويسنده , , T.S. and Golovin، نويسنده , , I.S. and Sinning، نويسنده , , H.-R. and Golovin، نويسنده , , S.A. and Siemers، نويسنده , , C.، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2006
Pages
7
From page
1238
To page
1244
Abstract
Anelastic effects in ternary Fe–Al–Si alloys at elevated temperatures (from 400 to ∼700 °C) have been studied by mechanical spectroscopy. The contributions of several damping mechanisms (high temperature background, Zener and grain boundary relaxations), which are sensitive to the structural state in the temperature range studied, are analysed. The structure of the alloys was examined by different methods. The results of computer analyses of the experimental data justify the superposition of several relaxation processes. Parameters of the Zener relaxation in two ternary Fe–Al–Si alloys are determined: the peak temperature is about 545 °C (f ≈ 2 Hz); the mean value of the activation energy of the Zener relaxation is about 2.54 eV.
Keywords
D. Defects: point defects , B. Order/disorder transformations , based on Fe3Al , A. Iron aluminides , A. Ternary alloy systems , B. Internal friction
Journal title
Intermetallics
Serial Year
2006
Journal title
Intermetallics
Record number
1503712
Link To Document