Damage of concrete experiencing flexural fatigue load and closed freeze/thaw cycles simultaneously
Author/Authors
Li، نويسنده , , Wenting and Sun، نويسنده , , Wei and Jiang، نويسنده , , Jinyang، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2011
Pages
7
From page
2604
To page
2610
Abstract
The damage evolution of concrete subjected to 4-point flexural fatigue load and closed freeze/thaw cycles simultaneously was experimentally studied. The responses on a separate fatigue load at 20 °C and −25 °C were tested to simulate the specimens with “thawed” or “frozen” pore water respectively. This damage, characterized by the residual strain, is 15.7% lower of the “frozen” state and 30.8% higher caused by the two loads than that of the “thawed” state. More interfacial cracking related signals were observed in the frequency domain using acoustic emission. The micrographys illustrate the cracks originate from the two damage sources, referring to the pores and the interfacial zones.
Keywords
Fatigue , Damage , Simultaneous , Freeze/thaw , combined
Journal title
Construction and Building Materials
Serial Year
2011
Journal title
Construction and Building Materials
Record number
1631526
Link To Document