Title of article
Formation of atomically smooth SiO2/SiC interfaces at ∼120 °C by use of nitric acid oxidation method
Author/Authors
Imai، نويسنده , , Shigeki and Fujimoto، نويسنده , , Masayuki and Asuha and Takahashi، نويسنده , , Masao and Kobayashi، نويسنده , , Hikaru، نويسنده ,
Issue Information
هفته نامه با شماره پیاپی سال 2006
Pages
4
From page
547
To page
550
Abstract
Conventional thermal oxidation of SiC requires heating at ∼1100 °C. In the present study, we have developed a method of oxidizing SiC at low temperatures (i.e., ∼120 °C) to form relatively thick silicon dioxide (SiO2) layers by use of nitric acid. When 4H-SiC(0 0 0 1) wafers are immersed in 40 wt% HNO3 at the boiling temperature of 108 °C and the boiling is kept for 5 h after reaching the azeotropic point (i.e., 68 wt% HNO3 at 121 °C), 8.1 nm thick SiO2 layers are formed on the SiC substrates. High resolution transmission electron microscopy measurements show that the SiO2/SiC interface is atomically flat and the SiO2 layer is uniform without bunching. When SiC is immersed in an azeotropic mixture of HNO3 with water from the first, the SiO2 thickness is less than 0.3 nm. The metal–oxide–semiconductor (MOS) diodes with the SiO2 layer formed by the nitric acid oxidation method possess a considerably low leakage current density.
Keywords
SiC , Nitric acid oxidation , Low temperature oxidation , Silicon oxides , NAOS , Insulating films
Journal title
Surface Science
Serial Year
2006
Journal title
Surface Science
Record number
1697677
Link To Document