Title of article :
Experimental study of static and fatigue strengths of pultruded GFRP rods bonded into LVL and glulam
Author/Authors :
Madhoushi، نويسنده , , Mehrab and Ansell، نويسنده , , Martin P، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2004
Pages :
7
From page :
319
To page :
325
Abstract :
Glass fibre-reinforced plastic (GFRP) pultruded rods were bonded into LVL and glulam cubes with room temperature cured epoxy resin in two glue-line thicknesses (2 and 4 mm). The strength properties were investigated under static and tension–tension (R=+0.1) fatigue loading. Also, the effect of rate of loading was assessed in a rate of force application range from 0.01 to 35 kN/s in three glue-lines thicknesses (0.5, 2 and 4 mm). The results demonstrate that the fatigue life increases as the peak dynamic load is reduced as expected. Better static strength is measured for 4 mm glue-lines than for 0.5 and 2 mm glue-lines at lower rates of loading, but a reduction in strength at higher rates is observed for 4 and 2 mm glue-lines. Glue-line thickness and rate of loading dictate the mode of failure observed including failure in timber, failure at the resin–rod interface and a mixed failure mode.
Keywords :
B. Wood , A. Epoxy , GFRP rod , D. Fatigue
Journal title :
International Journal of Adhesion and Adhesives
Serial Year :
2004
Journal title :
International Journal of Adhesion and Adhesives
Record number :
1698230
Link To Document :
بازگشت