Title of article
Production of mesophase carbon by PIM — Tailoring gel strength of agar binder
Author/Authors
Sommer، نويسنده , , Michael and Kellermann، نويسنده , , Karsten and Singer، نويسنده , , Robert F.، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2013
Pages
5
From page
228
To page
232
Abstract
This paper reports the results of a study on a water based binder with agar as a backbone for the production of carbon parts by powder injection moulding of carbon mesophase. The binder strength or gel strength of agar-binder is directly depended on the agar concentration in water and can be increased drastically by adding potassium tetraborate-4-hydrate. As the drying shrinkage of powder injection moulded samples is depending on the binder strength, brown and sinter density also increases with increasing agar and additive content. The packing density of samples increases from 60% (green) up to 83% (brown) during drying. By adding gel strengthening additives the agar content can be decreased and as this reduces the elusion of gaseous degradation products during thermal treatment debinding and sintering defects are eliminated. In this way stiffness of carbon material was increased from 7 MPa to 16 GPa.
Keywords
Powder injection moulding , Agar , Binder , carbon
Journal title
Powder Technology
Serial Year
2013
Journal title
Powder Technology
Record number
1703191
Link To Document