Title of article
Densification and microstructural development during sintering of powder injection molded Fe micro–nanopowder
Author/Authors
Choi، نويسنده , , Joon-Phil and Lyu، نويسنده , , Hyun-Gon and Lee، نويسنده , , Won-Sik and Lee، نويسنده , , Jai-Sung Lee، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2014
Pages
6
From page
596
To page
601
Abstract
The sintering behavior of the powder injection molded Fe micro–nanopowder fabricated under low temperature and low pressure conditions of 70 °C and 4 MPa was investigated in terms of the microstructural development. It was found that the sintered density of the micro–nanopowder was remarkably increased in the temperature range of 800 to 900 °C by the nanopowder effect due to the enhancement of the material transport by grain boundary diffusion. The micrograins in the micro–nanopowder almost maintained their initial grain size until the sintered density reached 90% of the theoretical density (TD), even showing no drastic grain growth under the condition of full density of 97% TD after sintering at 1250 °C for 3 h. This means that the presence of the nanopowders not only increases material transport paths for rapid densification but also suppresses the grain growth. The experimental findings in this study provide the potential application of micro–nanopowders for processing the PIM products with full density and fine microstructure.
Keywords
Powder injection molding , Micro–nanopowder , Sintering , microstructure , grain growth
Journal title
Powder Technology
Serial Year
2014
Journal title
Powder Technology
Record number
1704948
Link To Document