• Title of article

    The effect of pulse duration and oxygen partial pressure on La0.7Sr0.3CoO3−δ and La0.7Sr0.3Co0.2Fe0.8O3−δ films prepared by laser ablation

  • Author/Authors

    Waller، نويسنده , , David and Coccia، نويسنده , , Luigi G and Kilner، نويسنده , , John A and Boyd، نويسنده , , Ian W، نويسنده ,

  • Issue Information
    دوهفته نامه با شماره پیاپی سال 2000
  • Pages
    7
  • From page
    119
  • To page
    125
  • Abstract
    The effect of oxygen pressure and laser pulse duration on the production of thin films of La0.7Sr0.3CoO3−δ (LSC) and La0.7Sr0.3Co0.2Fe0.8O3−δ (LSCF) by laser ablation has been investigated. Evidence of reduction and phase separation of the target surfaces was found by X-ray diffraction. Ablation of LSC, at low oxygen partial pressures and with an excimer laser, led to the production of poor quality films, compared with the LSCF. This is attributed to the greater stability of LSCF in terms of low oxygen pressures.
  • Keywords
    Laser ablation , oxygen pressure , LSC , LSCF , Laser pulse duration
  • Journal title
    Solid State Ionics
  • Serial Year
    2000
  • Journal title
    Solid State Ionics
  • Record number