Title of article :
Esterification of ethylene-vinyl alcohol copolymers in homogeneous phase using N,N′-dimethylpropyleneurea as solvent
Author/Authors :
Fernلndez، نويسنده , , M.J. and Fernلndez، نويسنده , , M.D.، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2005
Pages :
11
From page :
1473
To page :
1483
Abstract :
Ethylene-vinyl alcohol copolymers (EVAL) were esterified with 3,5-dinitrobenzoyl chloride using the cycled urea N,N′-dimethylpropyleneurea (1,3-dimethyl-3,4,5,6-tetrahydro-2(1H)-pyrimidinone) (DMPU) as the solvent. Ethylene-vinyl alcohol-vinyl-3,5-dinitrobenzoate terpolymers (EVALVDNB) and ethylene-vinyl-3,5-dinitrobenzoate copolymers (EVDNB) were obtained. Both EVAL copolymers (6–73 mol% VAL) and esterified polymers, EVDNB, and EVALVDNB dissolve in DMPU. The substitution may become total under the experimental conditions. The degree of transformation was determined by 1H NMR. EVDNB copolymers were characterised by IR spectroscopy and 1H and 13C NMR. Thermal properties were studied by DSC. The glass transition temperature of the EVDNB copolymers having a low VDNB content (up to 14 mol%) is roughly constant, whereas above 50 mol% increases. Melting temperature decreases as the VDNB content is increased, owing to the fact that the VDNB groups are excluded from the polyethylene crystal lattice.
Keywords :
Ethylene-vinyl-3 , Ethylene-vinyl alcohol copolymers , 1 , 5-dinitrobenzoate copolymers , 3-Dimethyl-3 , 4 , 5 , 6-Tetrahydro-2(1H)-pyrimidinone
Journal title :
Polymer
Serial Year :
2005
Journal title :
Polymer
Record number :
1722650
Link To Document :
بازگشت