• Title of article

    Dynamic stress relaxation of thermoplastic elastomeric biomaterials

  • Author/Authors

    Puskas، نويسنده , , Judit E. and El Fray، نويسنده , , Miroslawa and Tomkins، نويسنده , , Matthew and Dos Santos، نويسنده , , Lucas M. and Fischer، نويسنده , , Frank and Altstنdt، نويسنده , , Volker، نويسنده ,

  • Issue Information
    دوهفته نامه با شماره پیاپی سال 2009
  • Pages
    5
  • From page
    245
  • To page
    249
  • Abstract
    In this paper we present the results of comparative dynamic stress relaxation studies performed with poly(styrene-b-isobutylene-b-styrene) (SIBS), polyurethane (PU) and polyester (PED) biomaterials in air and simulated body fluid (SBF) at 24 °C and 37 °C. SIBS showed the highest value of relieved stress under constant strain (24.1% after 100,000 cycles in air) with PED and PU having similar relative change (12.2% and 10.5%). In spite of its softness (Shore A 56 vs. 80), the dynamic modulus (Edyn) and stiffness of SIBS were in between PED and PU. The behavior of the materials was correlated to their structure: SIBS is an amorphous block copolymer with a long elastomer midblock, while PU and PED are semicrystalline segmented copolymers with much shorter soft blocks, and hydrogen bonding. SIBS and PED were relatively insensitive to SBF and temperature changes, while PU experienced the largest changes in physical properties in vitro (simulated body fluid, 37 °C).
  • Keywords
    Thermoplastic elastomers TPEs , Fatigue testing in vitro , Poly(styrene-b-isobutylene-b-styrene) block copolymer (SIBS)
  • Journal title
    Polymer
  • Serial Year
    2009
  • Journal title
    Polymer
  • Record number

    1732446