Title of article
Densification and microstructure of lead zirconate titanate ceramics fabricated from a triol sol–gel powder
Author/Authors
Sangsubun، نويسنده , , C. and Watcharapasorn، نويسنده , , A. and Jiansirisomboon، نويسنده , , S.، نويسنده ,
Issue Information
دوماهنامه با شماره پیاپی سال 2008
Pages
5
From page
61
To page
65
Abstract
Lead zirconate titanate (PZT) nano-powder was prepared by a triol sol–gel process. X-ray diffraction and transmission electron microscopy results showed that as-synthesized amorphous powder started to crystallize at the calcination temperature above 500 °C. The crystalline powder was formed into pellets and sintered at temperatures between 900 and 1300 °C. Co-existence of tetragonal and rhombohedral phase was observed in all ceramics. Microstructural investigation of PZT ceramics showed that uniform grain size distribution with average grain size of ∼0.8–2.5 μm were received with sintering temperature up to 1200 °C. Further increasing the temperature caused abnormal grain growth with the grain as large as 13.5 μm. An attempt to optimize densification with uniform grain size distribution was also performed by varying heating rate and holding time during sintering. It was found that dense (∼97%) sol–gel derived PZT ceramic with uniform microstructure was achieved at 1100 °C with a heating rate of 5 °C min−1 and 6 h dwell time.
Keywords
Sol–gel processes , Sintering , PZT
Journal title
Current Applied Physics
Serial Year
2008
Journal title
Current Applied Physics
Record number
1786058
Link To Document