    A low temperature synthesis of crystalline B4C ultrafine powders

  • Author/Authors

    Shi، نويسنده , , Liang and Gu، نويسنده , , Yunle and Chen، نويسنده , , Luyang and Qian، نويسنده , , Yitai and Yang، نويسنده , , Zeheng and Ma، نويسنده , , Jianhua، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2003
  • Pages
    3
  • From page
    5
  • To page
    7
  • Abstract
    B4C ultrafine powders were successfully synthesized at 450 °C through a new co-reduction route. The synthesis was carried out in an autoclave by using BBr3 and CCl4 as the reactants and metallic Na as the co-reductant. The X-ray powder diffraction pattern and Raman spectra indicate the formation of B4C. An atomic ratio of B to C of 4.09:1.0 was determined from X-ray photoelectron spectra. Transmission electron microscopy images shows that typical B4C crystallites are composed of uniform ultrafine spherical and rod-like particles.
  • Keywords
    C. X-ray diffraction , C. Transmission electron microscopy , B. Chemical synthesis , A. Boron carbide
  • Journal title
    Solid State Communications
  • Serial Year
    2003
  • Journal title
    Solid State Communications
  • Record number

    1788360