Abstract :
In this study, Cr12Mn2V2 high chromium cast iron (HCCI) was boronized at 900 °C and 950 °C for 2, 4, 6, and 8 h, respectively. The borided samples were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), microhardness tester and ring-on-block wear tester in terms of the phase composition, microstructure and worn surface morphology, microhardness, fracture toughness and abrasive wear resistance. The boride layer thickness ranges from 8 to 33 µm. XRD studies show the boride layer formed at 950 °C/8 h consists of the phases FeB, Fe2B and CrB, while for the layer formed at 900 °C/8 h, consists of mainly the Fe2B phase. Abrasive wear test results show that the relative wear resistance of the borided HCCIs increases with increasing surface microhardness.
Keywords :
High chromium cast iron , microstructure , Abrasion wear resistance , Boriding