Title of article
Effect of strength on environment-assisted cracking of Ti–8V–6Cr–4Mo–4Zr–3Al in aqueous NaCl: Part 1: Age hardening vs. work hardening
Author/Authors
Somerday، نويسنده , , B.P. and Gangloff، نويسنده , , R.P.، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 1998
Pages
13
From page
166
To page
178
Abstract
The objective of this research is to understand the effect of yield strength on the environment-assisted cracking (EAC) susceptibility of a β Ti alloy, Ti–8V–6Cr–4Mo–4Zr–3Al (Beta-C), precracked and stressed actively in aqueous NaCl. Isothermal aging renders immune, β-solution treated Beta-C susceptible to severe EAC coincident with strengthening by α precipitates. The threshold for EAC decreases to 40% of the air fracture toughness, subcritical crack growth rate approaches 100 μm s−1, and the crack path becomes fully intergranular for aging times in excess of several hours. In contrast, solution treated and cold-worked single-phase β Beta-C retains immunity to EAC for similar high strengths. For several levels of cold work, Beta-C cracks by transgranular microvoid processes, with equal values of EAC threshold stress intensity and air fracture toughness. Cold work reduces the air fracture toughness of β-phase Beta-C compared to values for β/α microstructures at similar strengths. The strength increase due to α precipitation does not uniquely promote EAC susceptibility.
Keywords
Environment-assisted cracking , Aqueous NaCl , HARDENING
Journal title
MATERIALS SCIENCE & ENGINEERING: A
Serial Year
1998
Journal title
MATERIALS SCIENCE & ENGINEERING: A
Record number
2138228
Link To Document