    Joining alumina/zirconia ceramics

  • Author/Authors

    Goretta، نويسنده , , K.C. and Gutierrez-Mora، نويسنده , , F and Picciolo، نويسنده , , J.J and Routbort، نويسنده , , J.L، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2003
  • Pages
    5
  • From page
    158
  • To page
    162
  • Abstract
    Dense compacts consisting of 40 vol.% Al2O3–60 vol.% 3 mol% Y2O3-stabilized ZrO2 (YSZ) were joined with an interlayer of 50 vol.% Al2O3–50 vol.% YSZ. A joint was also made at 1200 °C with an interlayer that was 50 vol.% Al2O3–50 vol.% ZrO2, in which the average particle size of both powders was ≤20 nm. The joint materials were applied by aerosol spraying, and thus the technique is suitable for commercial application. Superplastic deformation at 1200–1350 °C required ≤2 h to form fully dense joints in which minimal grain growth occurred. Virtually perfect joints were also made with various other ratios of Al2O3–YSZ.
  • Keywords
    ZrO2 , Al2O3 , Superplastic
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: A
  • Serial Year
    2003
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: A
  • Record number

    2141394