Title of article
Ferroelectric properties of ultrasonochemically prepared SbSI ethanogel
Author/Authors
Szperlich، نويسنده , , Piotr and Nowak، نويسنده , , Marian and Bober، نويسنده , , ?ukasz and Szala، نويسنده , , Janusz and Str??، نويسنده , , Danuta، نويسنده ,
Issue Information
فصلنامه با شماره پیاپی سال 2009
Pages
4
From page
398
To page
401
Abstract
This article presents for the first time the electrical properties of sonochemically synthesised, high-surface-area SbSI ethanogel made up of large quantity nanowires with lateral dimensions of about 10–50 nm and lengths reaching up to several micrometers. The composition, morphology, dimensions, microstructures, and optical energy gap of the new form of SbSI were characterized. This material is a semiconducting ferroelectric as in the case of bulk SbSI crystals. The maximum of dielectric constant ε = 1.6 × 104 is observed at Tc = 292(1) K. The activation energies in temperature dependences of electric conductivity of SbSI ethanogel are different for ferroelectric and paraelectric phases during heating and cooling of the sample.
Keywords
nanowires , Ferroelectrics , Sonochemistry , Semiconductors , Antimony sulfoiodide
Journal title
Ultrasonics Sonochemistry
Serial Year
2009
Journal title
Ultrasonics Sonochemistry
Record number
2189370
Link To Document