This paper seeks to outline the temperature effect on the buckling properties of ultra-thin-walled lenticular collapsible composite tube (LCCT) subjected to axial compression. The buckling tests of the LCCT specimens subjected to axial compression were carried out on INSTRON-500N servo-hydraulic machine in dry state and at the temperatures of 25 °C, 100 °C and −80 °C. The load–displacement curves and buckling initiation loads were measured and the buckling initiation mechanism was discussed from experimental observations. Experiments show that the buckling initiation load, on average, is only about 2.2% greater at the low temperature of −80 °C than at the room temperature of 25 °C due to the material hardening, demonstrating an insignificant increase in the buckling initiation load, whereas it is about 19.5% lower at the high temperature of 100 °C than at the room temperature owing to the material softening, implying a significant decrease in the buckling initiation load. The failure mode of the LCCT in axial compression tests at three different temperatures can be reckoned to be characteristic of the buckling initiation and propagation around the central region until rupture. The finite element (FE) model is presented to simulate the buckling initiation mechanism based on the eigenvalue-based methodology. Good correlation between experimental and numerical results is achieved.
Keywords :
Finite element analysis , Lenticular collapsible tube , Axial compression , Buckling , Composite
Journal title :
Chinese Journal of Aeronautics
Serial Year :
2014
Journal title :
Chinese Journal of Aeronautics
Record number :
2265698
Link To Document :
بازگشت