Abstract :
The wide scattering in tool life of natural mono-crystalline diamond tools is considered to depend on intrinsic crystalline defects due to nitrogen impurities in raw diamond. In this paper, the correlation was investigated between the amounts and types of the impurity evaluated by infrared absorption (IRA) and the crater wear and chipping resistances. As a result, diamonds including less total amount of impurity show larger wear resistance and that with larger amount of B2-aggregates show larger chipping resistance. This suggests that the inspection by IRA can be a useful method for screening of raw diamond for highly durable cutting tools.
Keywords :
turning , WEAR , diamond
Journal title :
CIRP Annals - Manufacturing Technology
Journal title :
CIRP Annals - Manufacturing Technology