Effects of Sc content on the microstructure of As-Cast Al-7 wt.% Si alloys
Author/Authors :
Zhang، نويسنده , , Wenda and Liu، نويسنده , , Yun and Yang، نويسنده , , Jing and Dang، نويسنده , , Jinzhi and Xu، نويسنده , , Hong and Du، نويسنده , , Zhenmin، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2012
Abstract :
The effects of Sc content on the microstructure of as-cast Al-Si alloys were investigated by adding 0.05, 0.1, 0.15, 0.2, 0.25, 0.3, and 0.4 wt.% Sc to hypoeutectic Al-7 wt.% Si alloys. The results show that there are significant changes in the microstructure when the Sc content is increased to 0.15%. The volume fraction of the primary α-Al phase increased nearly monotonically with increasing Sc content in the as-cast state. As the Sc content increased, the average length of the eutectic Si in the as-cast Al-7Si-xSc alloy decreased sharply from 150 μm (without Sc content) to 20 μm (0.4 wt.% Sc content). The Sc atoms are concentrated in the interdendritic regions. A fish-bone structure composed of Al, Si, Sc, and Fe, which might be the Fe-rich phase precipitated on the AlSc2Si2 (V-phase) was detected adjacent to the grain boundary by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS).
Keywords :
Al-Si alloys , Sc content , Grain refinement , modification
Journal title :
Materials Characterization
Journal title :
Materials Characterization