Title of article :
Pressure chloride leaching of a refractory gold ore
Author/Authors :
Pangum، نويسنده , , L.S. and Browner، نويسنده , , R.E.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 1996
Pages :
10
From page :
547
To page :
556
Abstract :
A series of metallurgical methods were employed to recover gold contained in a pyrite matrix. Direct cyanidation of the ore at P80 = 75 μm yielded only 33% recovery after 24 hours leach time. Efforts to improve this level of recovery by finer grinding to 53μm and 38 μm followed by subsequent cyanidation were fruitless. A maximum of 35% Au recovery was realised. e was then roasted at 650°C and the calcine was subsequently leached with cyanide. After 24 hours of leaching, 98% of the gold was recovered. Finally, the ore was treated by simultaneous oxidation and gold dissolution within an autoclave using a O2/H2SO4/HCl/NaCl system. The results revealed that at temperatures between 180–200 °C, between 1.5 to 2 hours was required to attain sulphide oxidation and attendant gold recoveries in excess of 90%. This system indicated the potential for direct dissolution of gold within the autoclave thus avoiding the need for cyanidation treatment of the autoclave discharge as is currently done.
Keywords :
Oxidation , Leaching , precious metal ores , sulphide ores
Journal title :
Minerals Engineering
Serial Year :
1996
Journal title :
Minerals Engineering
Record number :
2272614
Link To Document :
بازگشت