Title of article :
Nanoporous carbons from cypress I. Preparation and pore structure
Author/Authors :
Ito، نويسنده , , Eiki and Kouchi، نويسنده , , Ikuyoshi and Mozia، نويسنده , , Sylwia and Okuda، نويسنده , , Masaharu and Nakano، نويسنده , , Takashi and Toyoda، نويسنده , , Masahiro and Inagaki، نويسنده , , Michio، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2007
Pages :
7
From page :
199
To page :
205
Abstract :
Nanoporous carbons were prepared from cypress chips under a flow of super-heated steam, and their surface area reached more than 1000 m2/g without an additional activation process. Cypress charcoals prepared at a temperature of 800–870°C had a large external surface area of more than 400 m2/g, comparable to the microporous surface area, even though only 30–40 m2/g was obtained by carbonization in a flow of Ar gas. Cypress charcoals prepared above 900°C were microporous with a microporous surface area more than 800 m2/g and an external surface area of about 150 m2/g. The pore structure in cypress charcoals could be controlled by selecting the temperature of the steam.
Keywords :
microporous , carbonization , Mesoporous , Cypress charcoal , Super-heated steam
Journal title :
New Carbon Materials
Serial Year :
2007
Journal title :
New Carbon Materials
Record number :
2278036
Link To Document :
بازگشت