Abstract :
An age-hardened Al–Li–Cu–Mg–Zr alloy (AA8090) used for a substantial part of the structure of a helicopter (in order to save weight) exhibited low-energy intergranular fracture during accidents, resulting in extensive damage. With this experience in mind, various hypotheses for brittle intergranular fracture in Al–Li alloys are reviewed, and possible remedial measures outlined. The effects of variables such as alloy composition, ageing times and temperatures, crystallographic texture, and test temperature on brittle-intergranular-fracture resistance are described, and it is concluded that lithium segregation to grain boundaries is primarily responsible for brittle intergranular fracture. Lithium segregation occurs mainly during the primary ageing treatment; but secondary ageing during service, where temperatures can reach 50–80 °C, could increase lithium segregation and further increase susceptibility to brittle intergranular fracture. The evidence also suggests that the prevalence of a planar-slip-mode in Al–Li alloys, resulting in dislocation pile-ups at grain boundaries, is not responsible for brittle intergranular fracture, contrary to widespread opinion.
Keywords :
Aluminium–lithium alloys , Intergranular fracture , thermal stability , Grain-boundary segregation , Slip-mode
Journal title :
Engineering Failure Analysis
Serial Year :
2012
Journal title :
Engineering Failure Analysis
Record number :
2339514
Link To Document :
بازگشت