Gerami-Panah, F Department of Prosthodontics - Faculty of Dentistry - Tehran University of Medical Sciences, Tehran , Jalali, H Department of Prosthodontics - Faculty of Dentistry - Tehran University of Medical Sciences, Tehran , Sedighpour, L Department of Prosthodontics - Faculty of Dentistry - Tehran University of Medical Sciences, Tehran
Pages
9
From page
159
To page
167
Abstract
Statement of Problem: The connector area is the weakest zone of an all-ceramic fixed
partial denture (FPD), where most catastrophic failures of the prostheses tend to occur.
Purpose: The aim of the present study was to assess the effect of the convergence angle
of abutments on the fracture resistance of three-unit fixed partial dentures made of IPSEmpress2.
Materials and Methods: Forty extracted human premolars and molars were used to
reproduce twenty, 3-unit fixed partial dentures, for the replacement of second
premolars. All teeth were prepared according to the guidelines outlined for all-ceramic
crowns and bridges, except for the convergence angles of the abutments. The specimens
were randomly divided into two groups of 10, with total occlusal convergence angles of
12° and 22°. Fixed partial dentures with a uniform thickness of 0.8 mm were fabricated
using IPS-Empress2 and were bonded to the corresponding models. Connector
dimensions were set to 4 mm height and 4mm width. The radius of curvature at the
gingival embrasure was carved to 0.9 mm. All specimens were exposed to 10,000 preloading
cycles and a load of 40 N at a frequency of 1.3 Hz in a standardized testing
machine at a cross head speed of 1mm/min. Student t-test was performed to detect any
difference in the mean fracture resistance between the two groups (α = 0.05).
Results: Mean failure loads (and standard deviations) of the 12° and 22° groups were
1009.12 N (208.05) and 1182.72 N (144.67), respectively. Statistical analysis revealed a
significant difference (P <0.04) between the mean failure loads of the two groups. Most
fractures occurred through the connectors.
Conclusion: The mean failure loads of the investigated fixed partial dentures were
higher in the abutments with 22° taper as compared to those with a taper of 12°.
Farsi abstract
بيان مسأله: ناحيه اتصال ضعيف ترين نقطه در پروتزهاي ثابت تمام سراميك است كه مي تواند منجر به شكست هاي غير قابل جبران ايـن
پروتزها شود.
هدف: هدف از مطالعه حاضر ارزيابي اثر زاويه تقارب تراش دندان هاي پايه بر ميزان مقاومت به شكـست بـريج هـاي سـه واحـدي تمـام
سراميك است.
روش تحقيق: تعداد 40 دندان پرمولر و مولر انساني جهت بازسازي بيست بريج سه واحدي براي جايگزيني د ندان پرمـولر دوم انتخـاب
شدند. تمامي نمونه ها براساس دستورالعمل تراش دندان هاي پايه بريج هاي تمام سراميكي به جز از نظر زاويه تقـارب تـراش آمـاده شـدند .
نمونه ها به طور تصادفي به دو گروه با مجموع زواياي تقارب اكلوزالي 12و 22 درجه تقسيم شدند. پروتزهاي ثابت سـه واحـدي از جـنس
2 Empress-IPS با ضخامت يكنواخت 0/8 ميليمتر ساخته و بر روي دندانهاي پايه چسبانده شدند. عـرض و ارتفـاع ناحيـه اتـصال بـه
اندازه چهار ميليمتر ساخته شد. شعاع قوس امبرژور لثه اي در حد 0/9 ميليمتر درنظر گرفته شد.
در بارگذاري اوليه هر نمونه 10/000 بار تحت نيروي معادل 40 نيوتن با فركانس 1/3 هر تز قرار گرفتند و سپس توسط دسـتگاه آزمـون
استاندارد (Zuick (با سرعت head-Cross يك ميليمتر در دقيقه ميزان مقاومت به شكـست آنهـا انـدازه گيـري شـد. آنـاليز آمـاري -t
student جهت مقايسه مقاومت به شكست در دو گروه با درنظر گرفتن خطاي نوع اول آماري برابر 0/05 استفاده شد.
يافتـه هـا: ميـانگين مقاومـت بـه شكـست و انحـراف معيـار در گـروه 12 درجـه 208/05±10012/12 نيـوتن و در گـروه 22 درجـه
144/67±1182/72 نيوتن بدست آمد. اختلاف آماري بين اين دو ميزان معني دار بود (05/0
Keywords
Fixed partial denture , Fracture resistance , Dental ceramics , Lithium disilicate , All-ceramic , Glass ceramic , IPS-Empress 2