WAN KHODIR, WAN KHARTINI Universiti Kebangsaan Malaysia - Faculty of Science and Technology - School of Applied Physics, Malaysia , SHAMSUDIN, ROSLINDA Universiti Kebangsaan Malaysia - Faculty of Science and Technology - School of Applied Physics, Malaysia , DAUD, ABDUL RAZAK Universiti Kebangsaan Malaysia - Faculty of Science and Technology - School of Applied Physics, Malaysia , ABDULLAH, YUSOF Malaysian Institute for Nuclear Technology Research (MINT), Malaysia
From page :
77
To page :
80
Abstract :
Injectable biocement as bone substitute material for filling in parts of defect bone and capable of setting itself in the body was produced based on a mixture of 40-50% hydroxyapatite, 10-20% {3-tricalcium phosphate and 40-60% calcium sulphate dehydrate. Two different liquids were used for the preparation of the biocements, namely deionised water and phosphate buffer solution (pH 7). The influences of powder composition, weight ratio of liquid-to-powder and powder particle size on the injectability, setting time and compressive strength of the cement were reported.
Keywords :
Hydroxyapatite , Injectability, Compressive strength
Record number :
2554367
Link To Document :
بازگشت