S–N curve characteristics and subsurface crack initiation behaviour in ultra-long life fatigue of a high carbon-chromium bearing steel
Author/Authors :
K. SHIOZAWA، نويسنده , , L. Lu، نويسنده , , S. Ishihara ، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2001
Pages :
10
From page :
781
To page :
790
Keywords :
surface crack. , bearing steel , High cycle fatigue , non-metallicinclusion , S–N curve , internal crack , fish eye