• Title of article

    Lithiated short side chain perfluorinated sulfonic ionomeric membranes: Water content and conductivity

  • Author/Authors

    Walter Navarrini، نويسنده , , Bruno Scrosati، نويسنده , , Stefania Panero، نويسنده , , Alessandro Ghielmi، نويسنده , , Aldo Sanguineti، نويسنده , , Giuliana Geniram، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2008
  • Pages
    6
  • From page
    783
  • To page
    788
  • Abstract
    In view of possible applications as single-ion electrolyte for lithium batteries, some aspects of the lithium form of Hyflon Ion ionomer, a sulfonic short side chain (SSC) electrolyte, have been investigated. The synthesis of the ionomer and the successive membrane preparation is reported. An appropriate methodology for the direct salification of the ionomeric membrane from the SO2F form to lithium salt, using lithium hydroxide in absence of organic solvent has been found. Utilizing these SSC lithium ionomer membranes and though a particular methodology for the dehydration of the lithium ion membrane in non-aqueous media, it has been possible to achieve an ionic conductivity of 10−3 S cm−1 at room temperature [W. Navarrini, S. Panero, B. Scrosati, A. Sanguineti, European Patent 1,403,958 A1 (2003)]. Surprisingly it was observed that the membrane ionic conductivity depends on the dehydration methodologies adopted.
  • Keywords
    Short side chain ionomer , Lithium polymer electrolyte , Water content , Hyflon ion , Conductivity
  • Journal title
    Journal of Power Sources
  • Serial Year
    2008
  • Journal title
    Journal of Power Sources
  • Record number