Title of article :
Comparative study of Li[CrTi]O4, Li[Li1/3Ti5/3]O4 and Li1/2Fe1/2[Li1/2Fe1/2Ti]O4 in non-aqueous lithium cells
Author/Authors :
Kazuhiko Mukai، نويسنده , , Kingo Ariyoshi، نويسنده , , Tsutomu Ohzuku، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2005
Pages :
4
From page :
213
To page :
216
Abstract :
Comparative study of Li[CrTi]O4, Li[Li1/3Ti5/3]O4 and Li1/2Fe1/2[Li1/2Fe1/2Ti]O4 was carried out in order to understand zero-strain insertion mechanism. Degree of defect defined by the occupation of lithium ions at 16(d) sites in Fdimagem is 0% in Li[CrTi]O4, 17% in Li[Li1/3Ti5/3]O4 and 25% in Li1/2Fe1/2[Li1/2Fe1/2Ti]O4. Electrochemical tests in non-aqueous lithium cells indicated that no fatal damage was observed with respect to XRD even for 25% defect of spinel-framework structure based on lithium titanium oxides. All samples examined here show the character of so-called zero-strain lithium insertion materials while Li1/2Fe1/2[Li1/2Fe1/2Ti]O4 is converted to a rock-salt structure of Li3/2Fe1/2[Li1/2Fe1/2Ti]O4 in which Fe3+ ions at the tetrahedral sites move to the octahedral sites by changing oxidation state on reduction. FT-IR and Raman spectral measurements were also carried out and the factors affecting zero-strain insertion mechanism were discussed.
Keywords :
Lithium-ion battery , Lithium titanium oxides , Topotactic reaction , Zero-strain insertion materials
Journal title :
Journal of Power Sources
Serial Year :
2005
Journal title :
Journal of Power Sources
Record number :
445646
Link To Document :
بازگشت