Title of article :
Residual monomer content and its release into water from denture base materials
Author/Authors :
Pekka K. Vallittu، نويسنده , , Varpu Miettinen، نويسنده , , Pekka Alakuijala، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 1995
Abstract :
Objectives. The aim of this study was to determine the content and amount of residual monomer released from heat-cured and chemical-cured polymethyl methacrylate (PMMA) during storage in water.
Methods. Residual monomer was extracted from ground PMMA with tetrahydrofuran and from the storage water with n-hexan. Samples were analyzed by using HPLC-chromatography. Duration of the storage period in water was up to 8 wk at temperatures of +22°C and +37°C.
Results. Residual monomer content of chemical-cured PMMA was higher than that of heat-cured PMMA. The effect of storage temperature was significant (p<0.001). During the first day of storage at +37°C, the monomer release from chemical-cured PMMA was 1906.7 ppm and from the heat-cured PMMA 34.5 ppm and that release was higher at +37°C than at +22°C (p<0.001).
Significance. This study suggests that the amount of released monomer can be diminished by storing the PMMA product in water for at least 1 d before use, preferably at +37°C.