Title of article :
Graphite Application and Different Powers of Neodymium-Doped Yttrium Aluminium Garnet (Nd:YAG) Laser on Dentin Surface Changes: A Scanning Electron Microscopy Study
Author/Authors :
Birang، Reza نويسنده Department of Periodontology, School of Dentistry, Isfahan University of Medical Sciences , , Yaghini، Jaber نويسنده Department of Periodontology, School of Dentistry, Isfahan University of Medical Sciences , , Fakhari، Elham نويسنده Torabinejad Dental Research center and Department of Periodontic, School of Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran. , , Hasheminia، Seyed Mohsen نويسنده Torabinejad Dental Research center and Department of Endodontics, School of Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran. , , Mousavi، Maryam نويسنده School of Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran. , , Farhadzadeh، Mahnaz نويسنده School of Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran. , , Birang، Ehsan نويسنده Dentist, Private Practice, Isfahan ,
Issue Information :
فصلنامه با شماره پیاپی سال 2012
Pages :
7
From page :
153
To page :
159
Abstract :
Introduction: Various methods have been used for the treatment of dentine hypersensitivity such as dentifrices, sealants and different types of lasers. The aim of this study was to evaluate the effect of Neodimium:Yttrium-Aluminium-Garnet (Nd:YAG) laser in association with graphite on the dentin morphologic changes. Methods: In this experimental in vitro study, 16 freshly extracted third molars were selected. 5 specimens with the dimensions of 2×2×1 mm from root trunk were prepared. Specimens were randomly divided into five groups: group 1 (control, no laser irradiation). Group 2, 3 irradiated by Nd:YAG laser 0.5 and 1W, output power respectively. Group 4, 5 smeared with graphite and then irradiated by Nd: YAG laser 0.5 and 1W output power. Samples were prepared for scanning electron microscopy. Number and diameter of dentinal tubules were determined in different groups and analyzed with the Kruskal-wallis and Mann-Whitney tests (SPSS 16). Results: The number of tubules had significant difference between all groups (P < 0.001), except group 1 in comparison with group 2 (P > 0.05), and group 3 in comparison with group 4 (P > 0.05). Micro-cracks and rupture of melted dentin materials were seen in group 4 and 5. Conclusion: According to the findings of this study, smearing with graphite on dentin surface increase the absorption of Nd:YAG laser energy and reduced the diameter and number of open dentinal tubules.
Journal title :
Journal of Lasers in Medical Sciences
Serial Year :
2012
Journal title :
Journal of Lasers in Medical Sciences
Record number :
682480
Link To Document :
بازگشت