Title of article :
Recovery of nickel oxide from spent catalyst
Author/Authors :
N. M. Al-Mansi، نويسنده , , N. M. Abdel Monem، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2002
Pages :
6
From page :
85
To page :
90
Abstract :
This study investigates the possibility of recovering nickel from the spent catalyst (NiO/Al2O3) resulting from the steam reforming process to produce water gas (H2/H2O) in many industries. In the extraction process, nickel is recovered as sulfate using sulfuric acid as a solvent. The considered parameters affecting nickel recovery were acid concentration, temperature and time of digestion solid:liquid ratio, particle size and stirring rate. Nickel was to be directly recovered as a sulfate salt by direct crystallization method. The conversion was 99% at 50% sulfuric acid concentration, solid: liquid ratio (1:12) by weight, particle size less than 500 micron for more than 5 h and 800 rpm at 100°C.
Keywords :
Spent catalyst , Nickel oxide , Nickel recovery , Leaching
Journal title :
Waste Management
Serial Year :
2002
Journal title :
Waste Management
Record number :
774627
Link To Document :
بازگشت