Abstract
Yttria stabilized zirconia (7YSZ) solution precursor
has been successfully used in the deposition of high
durability thermal barrier coatings. In this paper, the thermal
and crystallization behaviors of 7YSZ precursor were
investigated by TG-DTA, FTIR and XRD. The results show
that the precursor decomposition and crystallization temperatures
greatly depend on heating rate e. g. 74 C for the
crystallization temperature when tripping the heating rate.
With a 10 C/min heating rate, the weight loss due to precursor
pyrolysis occurs predominantly at temperatures below
500 C. A small weight loss due to the oxidation of
residual carbon is detected from 800 C to 950 C. The
complete crystallization of the tetragonal phase was determined
to be around 500 C by DTA and XRD analyses with
a 10 C/min heating rate. The crystallization kinetics and
the activation energy of amorphous 7YSZ precursor were
investigated by variable heating rate DTA. The calculated
activation energy is 66.2 kJ/mol. The Avrami parameter
value was determined to be 2.68, which indicates that
crystallization nucleation and growth is diffusion-controlled.
The crystalline phase of 7YSZ coatings deposited
by the Solution Precursor Plasma Spray process was identified
by XRD and Raman spectrum. The average YSZ grain
size in the SPPS coating was determined to be 61 nm.