Abstract :
Investigation of fracture toughness on Ti-6.5Al-
2Zr-1Mo-1V alloy thin sheet and its laser-welded joints has
been carried out. In the test compact tension (CT) specimens
and single specimen technology were used. In addition,
hardness distribution and microstructure of the welded
joints were examined. Fracture test indicates that brittle
unstable fracture occurs after slow crack propagation for all
the specimens, except that one heat affected zone (HAZ)
specimen is brittle crack initiation. It is found that rolling
directions have no obvious effect on fracture toughness of
base metal. Moreover, fracture toughness of weld metal is
obviously decreased in comparison with base metal whatever
in as-welded condition or in stress relief condition.
Post-weld heat treatment (PWHT) leads to fracture toughness
of the welds further decreasing. Fractography observation
shows that the fracture mode is predominantly
dimpled in base metal. However, there exists intergranular
fracture in the weld metal. Thus, the transition of fracture
mode from both base metal and HAZ to weld metal may
lead to dramatic decrease in fracture toughness. Microstructure
examination reveals that the microstructure of
weld metal consists of large grains with fine acicular
structure. The formation of fine a acicular structure is due to
rapid cooling during laser welding. After PWHT, the acicular
structure is coarsened.